Weiser, P.S.; Prawer, S.
Melbourne Univ., Parkville, VIC (Australia). School of Physics1995
Melbourne Univ., Parkville, VIC (Australia). School of Physics1995
AbstractAbstract
[en] When Fe is exposed to the plasma environment suitable for the chemical vapor deposition (CVD) of diamond, the surface is rapidly covered with a thick layer graphitic soot and C swiftly diffuses into the Fe substrate. Once the soot reaches a critical thickness, diamond films nucleate and grow on top of it. However, adhesion of the film to the substrate is poor due to the lack of structural integrity of the soot layer, A thin coating of TiN on the Fe can act to prevent diffusion and soot formation. Diamond readily grows upon the TiN via an a-C interface layer, but the a-C/TiN interface is weak and delamination occurs at this interface. In order to try and improve the adhesion, the use of a high dose Ti implant was investigated to replace the TiN coating. 7 refs., 6 figs
Source
1995; 13 p
Record Type
Report
Literature Type
Numerical Data
Report Number
Country of publication
Reference NumberReference Number
INIS VolumeINIS Volume
INIS IssueINIS Issue