AbstractAbstract
[en] The dissolution amount of Zn plate was 0.058 mg/cm2 in the non-magnetically treated solution, and was 0.059 mg/cm2 in the magnetically treated solution after 24 hour of immersion. The magnetic treatment had no effect to corrosion of Zn plate as pH on surface was not recognized the difference. The addition of Zn(II) ion in the solution was prepared to the effects of corrosion and dissolution of Fe. The regularity was not obtained the effect of the magnetic treatment on the dissolution of Fe plate
Primary Subject
Source
8 refs, 16 figs
Record Type
Journal Article
Journal
Corrosion Science and Technology; ISSN 1598-6462; ; v. 5(2); p. 39-44