Magnetic cluster mean-field description of spin glasses in amorphous La-Gd-Au alloys
Poon, S.J.; Durand, J.
California Inst. of Tech., Pasadena (USA). W.M. Keck Lab. of Engineering Materials1978
California Inst. of Tech., Pasadena (USA). W.M. Keck Lab. of Engineering Materials1978
AbstractAbstract
[en] Bulk magnetic properties of splat-cooled amorphous alloys of composition La/sub 80-x/Gd/sub x/Au20 (0 less than or equal to x less than or equal to 80) were studied. Zero-field susceptibility, high-field magnetization (up to 75 kOe) and saturated remanence were measured between 1.8 and 2900K. Data were analyzed using a cluster mean-field approximation for the spin-glass and mictomagnetic alloys (x less than or equal to 56). Mean-field theories can account for the experimental freezing-temperatures of dilute spin-glasses in which the Ruderman-Kittel-Kasuya-Yosida interaction is dominant. For the dilute alloys, the role of amorphousness on the magnetic interactions is discussed. By extending the mean-field approximation, the concentrated spin-glasses are represented by rigid ferromagnetic clusters as individual spin-entities interacting via random forces. Scaling laws for the magnetization M and saturation remanent magnetization M/sub rs/ are obtained and presented graphically for the x less than or equal to 32 alloys in which M/x = g(H/x*, T/x), M/sub rs/(T)/x = M/sub rs/(0)/x/ exp (-α*T/x/sup p/) where x* is the concentration of clusters, α* is a constant, and p is the freezing-temperature exponent given by T/sub M/ infinity x/sup p/. It is found that p = 1 and 1.3 for the regions 4 less than or equal to x less than or equal to 40 respectively. An attempt is also made to account for the freezing temperatures of concentrated spin glasses. The strength of the interaction among clusters is determined from high-field magnetization measurements using the Larkin-Smith method modified for clusters. It is shown that for the x < 24 alloys, the size of the clusters can be correlated to the structural short-range order in the amorphous state. More concentrated alloys are marked by the emergence of cluster percolation
Primary Subject
Source
Mar 1978; 52 p; Available from NTIS., PC A04/MF A01
Record Type
Report
Report Number
Country of publication
Descriptors (DEI)
Descriptors (DEC)
Reference NumberReference Number
INIS VolumeINIS Volume
INIS IssueINIS Issue