Stringing Pre-padding: Pipeline crossing angle: FBE Coating Application: (Fusion Bonded Epoxy)

Stringing:

  • Non-metallic, non-abrasive slings

Pre-padding:

  • Only dune sand (fine sand) having a particle size of less than 3.00 mm

Pipeline crossing angle:

  • The crossing of existing pipelines, cables, power lines, roads, railways, and waterways should be at an angle between 60° and 120°, but in no case shall the angle be less than 30°.

FBE Coating Application: (Fusion Bonded Epoxy)

  • FBE Inspection: Visual inspection, foam void test, cure test, adhesion test, film thickness measurement, impact test, holiday detection test

Shrink Sleeve Application:

  • Visual inspection
  • Adhesion test

To view or add a comment, sign in