Did you see our “Breakage of Refillable Bottles” Case Study in our Q4 e-Newsletter? If not, read it here: https://lnkd.in/gKgTR7Xm #glasspackaging #beverageindusdry #glassindustry
Bu vakada doldurulabir şişenin kırılma sebebi,dipteki yaralı tampon veya alt gravür 'ler arası küçük çatlak olur.Buda dolum esnasında basınç mukavemetine dayanamayıp kırılmaya sebeb verir.
Should not of made it to the consumer!
Glass
1moMany years ago we changed to turbine stipple to fix stipple checks and impact breakage with success not sure if this would help